You can refer to Caustic service graph given in API 571, Damage Mechanisms. It is given under topic of Caustic Embrittlement/caustic SCC.
Carbon steel is widely used for this service, however at certain temperature MOC's are upgraded.

thanks n regards,

Nishant Nair
Senior Engineer Reliability

Sent from Yahoo Mail on Android
From:"Chetan" <patilvicky4@gmail.com>
Date:Mon, 16 Nov, 2015 at 14:20
Subject:[MW:23885] MOC for CAUSTIC service

Dear all,

Please guide to selection of Moc for caustic Service.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1447664575.51633.YahooMailAndroidMobile%40web142504.mail.bf1.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...