Sunday, November 15, 2015

Re: [MW:23879] Pressure test Tolerance

Dear,

If it is a piping pressure test refer API 570,
If Vessels pressure test Refer API 510.

Regards

On Sun, Nov 15, 2015 at 5:38 AM, pras ari <alhanif.pras@gmail.com> wrote:
Dear Expert,

We want submit pressure test to Client, please advise to me about How much maximum pressure drop / down which allowable in pressure test at site?

Thanks & Regards
Winarko

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMoAFwoXWjUG76i9aNq8aKDBjPg%2BWS_B8%2BmPVzTbMY8JieBURg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Thanks and Regards, ?

Mohammed Ghani,

CSWIP 3.1 / BGAS L-2 / ISO 9001:2008 QMS LA.

Mechanical Inspector,
BUREAU VERITAS.


ü
 Please consider the environment before printing this email.

 "Be the change you wish to see in the world"

---Mahatma Gandhi---

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVjCdg600KprH%3Dm0GQtdEKnYx3no2LWBEy1S%2B%2B5SxXY_%2BQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...