Sunday, November 15, 2015

[MW:23877] Re: Pressure test Tolerance

you are doing inservice hydro test refer API570.

On Sunday, November 15, 2015 at 7:38:54 AM UTC+3, pras ari wrote:
Dear Expert,

We want submit pressure test to Client, please advise to me about How much maximum pressure drop / down which allowable in pressure test at site?

Thanks & Regards
Winarko

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b1daf153-7d86-4a3c-9f74-d6d63965eb21%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...