RE: [MW:23616] Fillet weld

Dear Mr. Poojary,

QW-202.2(c) says:
''Qualification for Fillet Welds. WPS qualification for fillet welds may be made on groove-weld test coupons using test specimens specified in (a) or (b). Fillet-weld procedures so qualified may be used for welding all thicknesses of base metal for all sizes of fillet welds, and all diameters of pipe or tube in accordance with Table QW-451.4. Nonpressure-retaining fillet welds, as defined in other Seetions of the Code, may as an alternate be qualified with fillet welds only. Tests shall be made in accordance
with QW-180. Limits of qualification shall be in accordance witb Table QW-451.3.''

Table QW-451.4 Fillet Welds Qualified by Groove-Weld Tests shall also be considered.

Best regards

Parvan Chavdarov

Dr.-Ing. Parvan Chavdarov
ASME A, B & N Inspector,IWE
Business Unit Nuclear Safety

TÜV Rheinland Industrie Service GmbH
Am GrauenStein
51105 Köln
Tel.: + 49 221 806 4251
Fax: + 49 221 806-3402
Mobile: + 49 151 53171362
parvan.chavdarov@de.tuv.com

----- Цитат от Jay Poojary (jayogini@gmail.com), на 28.09.2015 в 17:18 -----

Dear Experts,
 
As per ASME, Welder is qualified to weld fillet joint, if he is qualified on groove joint. My question is -------------

 Wps approved for groove joint is applicable for fillet joint?

  If so where it is stated.

cordially,
Jay Poojary

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAcO%3DySZQkp22fraccZK2Eohv1k-CisD_Z2_p7XssaRAf9YEaw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



Dr.-Ing. Parvan Chavdarov



ASME A, B & N Inspector, IWE



Business Unit Nuclear Safety



 



TÜV Rheinland Industrie Service GmbH



Am Grauen Stein



51105 Köln



Tel.: + 49 221 806 4251



Fax: + 49 221 806-3402



Mobile: + 49 151 53171362



parvan.chavdarov@de.tuv.com



-------------------------------------
Mail.BG: Безплатен e-mail адрес. Най-добрите характеристики на българския пазар - 20 GB пощенска кутия, 1 GB прикрепен файл, безплатен POP3, мобилна версия, SMS известяване и други.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da02beb08b6ab2a70f0154fd0c5967d6.mailbg%40mail.bg.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...