Tuesday, September 29, 2015

Re: [MW:23582] Fillet Welds Qualified by Groove-Weld Tests

The WPS is not approved. The WPS is qualified based on a PQR.
A WPS has always to be revised in order to give direct guidance to the welder to perform a specific work.
If the revised WPS is covered by an existing PQR it is OK.
If not, a new PQR has to be issued

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Raghuram Bathula ---29/09/2015 07:43:16---Refer Table QW-451.4 of ASME BPV IX On 28 September 2015 at 19:18, Jay Poojary <jayogini@gmail.com>

From: Raghuram Bathula <raghurambathula@gmail.com>
To: Materials-Welding <materials-welding@googlegroups.com>
Date: 29/09/2015 07:43
Subject: Re: [MW:23578] Fillet Welds Qualified by Groove-Weld Tests
Sent by: materials-welding@googlegroups.com





Refer Table QW-451.4 of ASME BPV IX


On 28 September 2015 at 19:18, Jay Poojary <jayogini@gmail.com> wrote:
    Dear Experts,
     
    As per ASME, Welder is qualified to weld fillet joint, if he is qualified on groove joint. My question is -------------

     Wps approved for groove joint is applicable for fillet joint?

      If so where it is stated.

    cordially,
    Jay Poojary

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to
materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CADxVub%3DcLZX0u-GzJk5PCY%3DVVtrqbUBrP7QB%3DygEWgMBi7UF2g%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com