Re: [MW:23578] Fillet Welds Qualified by Groove-Weld Tests

Refer Table QW-451.4 of ASME BPV IX


On 28 September 2015 at 19:18, Jay Poojary <jayogini@gmail.com> wrote:
Dear Experts,
 
As per ASME, Welder is qualified to weld fillet joint, if he is qualified on groove joint. My question is -------------

 Wps approved for groove joint is applicable for fillet joint?

  If so where it is stated.

cordially,
Jay Poojary


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVub%3DcLZX0u-GzJk5PCY%3DVVtrqbUBrP7QB%3DygEWgMBi7UF2g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...