Tuesday, September 29, 2015

[MW:23590] Hardness without pwht

Dear sir,
We can do hardness prior to pwht. Please go ahead and do it without any hesitation and cross check it with given table.
Also in some cases we can exempt pwht if hardness value finds within range. For this please refer ASME code.
Thanks and regards,
Sombir

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5e34cac1-3775-4147-bb43-5de7165d87b3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...