[MW:23290] Carbon pick-up in stainless steels

A manufacturer of stainless steel pipes uses coal gas in reheating furnace to heat SS billets before the piercing operation. The coal gas is generated by combustion of coal in a hearth before the reheating furnace and 'simply filtered' before entry for combustion in the reheating furnace.

Is there any possibility of carbon pick-up in the billet due to the gas and other carried over products of combustion like tars etc, especially if the billet is of low carbon type?

Thanks in advance for your responses.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a5d3ee35-f1cd-478b-ba7b-74e1030b2bfb%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...