Dear sir, 

    Copper coating used in GMAW for electrical conduction purpose. Wire is directly connected to power source as it is used like electrode. But in GTAW it is for protective coating ( to prevent from rust or moisture). It is used as filler wire which is provided additionally.

Thanks & regards,
Chirag sandhane

On Friday, July 17, 2015, José Juan Jiménez Alejandro <jjjimeneza@gmail.com> wrote:
By the way you describe it may be that this is due to the contribution they are using, in many cases the contributions bring a copper coating, as this helps the electrical conductivity, it is very common to see this situation in fillet welds made with the GMAW process, the welding surface like waste oil or honey appreciated, "drops" are seen along the steak, but the picture that you are sending is not very clear, has no HD.
Regards.

2015-07-17 2:27 GMT-05:00 Pawan Tiwari <pawan.tiwari@dwekam.org>:

Dear Experts,

 

Kindly refer the attached job of eco coil of Boiler in tube to tube joint welding application.

During GTAW welding with ER70S-2 grade filler wire we have noticed liquid type impurities on weld bead.

Why such type of defects are coming?

Is it product defect or welding process defect?

Please support & share your views to move in right direction.

 

Thanks & Best regards

PT

 

 

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/55a8adfd.eabb420a.30ad2.ffff9552SMTPIN_ADDED_BROKEN%40gmr-mx.google.com.
For more options, visit https://groups.google.com/d/optout.



--

Ing. Jose Juan Jimenez Alejandro

Cel. 8116171750

Skype: jjjimeneza

--
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/lsbRq-vnNzw/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurJujh_pJZy9ckYMeCeV-qWFpwgKqCB1nLNPcWugsYZitg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADP96MTo3nZwoms06VAk3%3DkJn7QCOqv-kiZaPL5P4Wk4203Ezw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...