We have to weld A-240 TP 409 to A-240 TP 409 ( P-7 to P-7  Material ) & which Filler we can use ER 309L /ERNiCr-3.
Temperature is around 300 degree centigrade ( HRSG Bottom area this material is coming ) where this wps will be used.
Thanks in advance
Regards
Pradip

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8kd5BZtnMBjaza5GytD9s5VfyD%2BqLzXATNZQi6DGEZSKw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...