There are two type welding involve in Hadfield Steel(12-14% Mn steel or its alloy).

1)Joining of two similar grade (HADFIELD TO HADFIELD) OR DIFFERENT GRADE (HADFIELD TO OTHER GRADE STEEL).

2) Overlaying on Hdfield steel.

For joining of Hadfield to Hadfield or overlaying on headfield - We have to take care ony IPT. For this we can be used any water cooling arrangement as per job geometry.
 
For dissimilar welding we have to takecare material properties and welding behaviour of both material . We are enclosing very interesting youtube clip (Welding of Hadfield to EN-31 material). During welding we were trying to cooldown Hadfield , while for EN31 material we were maintaining PHT and IPT up to 250 digree C.


Thanks
Vinay Tripathi
+919643886124(India)


https://www.youtube.com/watch?v=X-RYRnDx4Lg






On Sunday, July 5, 2015 at 8:19:08 PM UTC+5:30, Hrushikesh Sangamnerkar wrote:

Hi..
Anyone has experience of welding Hadfield steel?

Hrushikesh H Sangamnerkar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c20970c7-f1f6-46f2-9ff6-15db593c768c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...