This is not a Code requirement. 

 

If I remember correctly, this originated from EPRI recommendations for 91 fabrication.  It typically appears in customer specifications/requirements.  If low hydrogen procedures&practices are followed and proper storage is maintained, the requirement is, in my opinion and experience, totally unnecessary.  If the forgoing are not properly attended to, 2 weeks maybe far too long a time period.

 

Others may disagree.  However my 20 years of fabrication experience have shown my statement to be correct.

 

Enjoy - John

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of pradip kumar Sil
Sent: Monday, May 18, 2015 6:52 AM
To: materials-welding
Subject: [MW:23297] Welding & pwht time difference in P-91 Material

 

Dear All,

Can anybody inform code reference in B-31.1 welding & pwht time diference. Client is asking for 14 days.

Is it mandatory in code

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3D5YTF7j9_HXs5PJzN2GMNjA8qZrrEAti7aO8ca4bCWTg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...