Sunday, May 10, 2015

Re: [MW:23259] Max.Base metal thickness qualified

No I already hv this PQR

Hrushikesh H Sangamnerkar

On May 9, 2015 11:35 PM, "Mohit Aggarwal" <aggarwalmohit05@gmail.com> wrote:

Are you qualifying PQR with taper on one side of higher thickness i.e. 40 mm.

Best Regards,
Mohit Aggarwal.

On 05-May-2015 5:51 pm, "Hrushikesh Sangamnerkar" <hrushi612@gmail.com> wrote:

Dear experts,
I have a P8 # P43 PQR.
Joint design = Single V
Base metal thickness for P8 = 40mm and for P43 = 20mm.
What should be the Max.Base metal thickness range qualified for such joint?

Regards,
Hrushikesh H Sangamnerkar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2oHcKgDYmxWs9gVLaM8WLSSCewN4XcECCjVs6i8fkr7jw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPNyF3xTa-YFhKEqaC_1ixrNH%2BShPV-5m%2Bc2bH%3DcyFCERg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2rFz-6%2BSb4hag5nXUZnWdXnf4Noi871wX1AocTuCFSPoA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...