Re: [MW:23006] WPS with groove welding will also qualify Fillet welding.


Agreed with Dr. Georgious,

This is listed as non essential Variable in ASME section IX.
Please refer QW : 4.2.30 

Regards,

Anosh Wankhade

From: george.dilintas@gr.bureauveritas.com
Sent: Thu, 21 May 2015 16:54:53
To: materials-welding@googlegroups.com
Subject: Re: [MW:23005] WPS with groove welding will also qualify Fillet welding.

When ASME is the Code, yes
This is not the case for EN 15614-1

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for Mohammed Ghani ---21/05/2015 13:13:43---Dear Experts, Can any one suggest if Groove welding WPS will Mohammed Ghani ---21/05/2015 13:13:43---Dear Experts, Can any one suggest if Groove welding WPS will also allow welding with

From: Mohammed Ghani <ghani386@gmail.com>
To: materials-welding@googlegroups.com
Date: 21/05/2015 13:13
Subject: [MW:23002] WPS with groove welding will also qualify Fillet welding.
Sent by: materials-welding@googlegroups.com





Dear Experts, 

Can any one suggest if Groove welding WPS will also allow welding with fillet. please guide with reference standard clause.

--
Thanks and Regards, ?

Mohammed Ghani,


CSWIP 3.1 / BGAS L-2 / ISO 9001:2008 QMS LA.

Mechanical Inspector,
BUREAU VERITAS.


ü
 Please consider the environment before printing this email.
 "Be the change you wish to see in the world"
---Mahatma Gandhi---

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to
materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAG7AWVjjPwZ%2BkvBBQ-mQ1p1XV0tjtSv4jh8vqu-icwtVMpD%2B7g%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OFE44D54DE.B3B1B3E4-ONC2257E4C.003EA35C-C2257E4C.003EB065%40LocalDomain.
For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1432207493.S.24917.13610.f4-235-222.1432271486.12684%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...