[MW:23039] Heat Analysis Requirements

Dear All,
            We all know that ASTM 105 & ASTM A 234 have their own General requirements given in ASTM A 960, A 961 etc. which should also be addressed along with original Product requirements. 

Now as per A 960/ 961 : Heat Analysis : "An Analysis of each heat of steel shall be made by the manufacturer to determine the percentage of those element specified in the individual product specification. If secondary melting process are employed, the heat analysis shall be obtained from one re-melted ingot of each Primary melt. The chemical Analysis thus determined shall conform to the requirements of the individual product specification. Note that Product Analysis(Check analysis) tolerances are not to be applied to the heat analysis requirements." 
Product Analysis: If a Product Analysis is performed, it shall be in accordance with Test Methods, Practices & Terminology A 751.

I have following questions for the above.

1. I want to know what exactly A 960/961 wants to say for "Black Highlighted-Underlined Part of "Heat Analysis". What is Primary & Secondary Melting Processes???
2. I have TCs of ASTM A 105 & ASTM A 234, which are only having Product Analysis. They don't have "Heat Analysis" Can we say that it is totally conforming to A 105 & A234?? As far as I can understand "Heat Analysis" is Mandatory for materials having this both Grades, "Product Analysis" is optional. m I right????

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3f3c0aef-2132-4f72-b09f-560b60d814f0%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...