Re: [MW:23156] J groove bevel end requirement

I believe the joint design preparation is more dependable on the type of the selected welding process, targeted mechanical properties and structural application.

Regards

Noé

On Tuesday, April 21, 2015, Prabhakar Raj <prabhakarmet@gmail.com> wrote:

Can anyone give me code reference for J groove bevel end  requirement above 22mm wall thickness.  Is it mandatory to go for J groove.?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B-71w9oYr_5Wb2e8MxKXSn_oWGa2YDv%2BQkOheTDE-D_ZoYRgA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEGUTtVW6GWam%3Dx-SEjbspGZtsRNtR%2BvBO1BkyBUFPbhwGEi_Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...