Tuesday, April 21, 2015

[MW:23135] 2160 PSI - Reparing Separator 2" Nozzles

Dear Experts,

Greetings..

Kindly advice which type of welding procedure & heat treatment for 2", Sch 160  nozzle pipe end joining with 75 mm thick carbon steel body Separator. 

Please reply with Pre heating temperature, Intervals of Heating, PWHT Procedures, Welding Rods Details


Thanks in Advance..

Williams.


Pictures attached for your reference.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ7fysvWYxFHv9cp%3DL%2B-gneiAU0TXosY031wXTaEjuErNg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...