The certificate must match the requirement of a batch with Qty or any other means to correlate. It cannot be any certificate unrelated to the actual product/s.
By the way we dont like to throw at you. We will politely give you. ( pun intended)

Rgds
G.Prakash
AIS, AIA LLC TX, USA
Technical Director, Hitek Engg Services, Dubai
 gprakash31@gmail.com.
Tel: +9714 2778511 Mob:+97152 979 5678

On Wed, Mar 4, 2015 at 1:22 PM, Vadivel Mahadevan <vadivelmahadev@gmail.com> wrote:
Dear Experts,

Can you please throw me an Idea whether we need to match the Quantity for EN10204 2,2 Certificates. 
Supposedly consider a lot of around 30 nos of a pressure part where customer has requested for EN 10204 2.2 Certification for internals. Whether I am supposed to submit him internals Test certificate to match this 30 nos or a sample TC is sufficient enough.

What is the procedure to raise this issue to EN body?

Thanks and regards
Vadivel. M

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1631183a-cb20-4d72-82bc-197dd5948d32%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUP4qLjQsZxt8Ys8CcApO4et0d082di0NFoKW74UHnOvd_69g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...