Sunday, March 22, 2015

[MW:22995] Fillet Weld Size

Dear All,

Please share your opinions  for calculating of fillet weld size of following:

a. As per ASME  B31.3 for same thickness and also different thicknesses with concave and convex shape.

b. As per AWS D1.1 or same thickness and also different thicknesses with concave and convex shape.

Regards,

Srinu

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABGg_FK%3DOn8Nr%2BFfKHosU6iZ28yZ5VdzhGXr3rgiWnscd7af7A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...