Wednesday, February 18, 2015

Re: [MW:22901] Excess penetration measurment in Radiograph

These all are the reasons, evaluation of excess penetration using RT for pipes, is never referenced in any codes.

ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,

Nandesh Kumar Arasappa

P.S. : Please don't print this e-mail unless you really need to.

--------------------------------------------
On Wed, 18/2/15, S.Mohammed <mohd52100@gmail.com> wrote:

Subject: Re: [MW:22899] Excess penetration measurment in Radiograph
To: materials-welding@googlegroups.com
Date: Wednesday, 18 February, 2015, 5:45 PM

from where to arrange
ball?

is there standard
size available?

--
You received this message because you are
subscribed to the Google Groups "Materials &
Welding" group.
To unsubscribe from
this group and stop receiving emails from it, send an email
to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/77bec4cf-1331-47d0-acd4-2011d230fc2e%40googlegroups.com.
For
more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1424277311.91425.YahooMailBasic%40web193606.mail.sg3.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...