Re: [MW:22893] Excess penetration measurment in Radiograph

Hi,

My opinion, in DWSI superimpose, you can see the excess penetration clearly. Please refer the attached image.

Please refer table 341.3.2 for acceptance criteria. However as Mr. Jerald mentioned earlier you can go for ball passing test to confirm the ID.


regards,
LALU
LINKS MIDDLE EAST
ABU DHABI, UAE

On Wed, Feb 18, 2015 at 12:19 AM, sundarrajan kumaraswamy <ksraja15@gmail.com> wrote:
  How to measure the excess penetration from the Radiograph of Small bore piping  DWDI superimpose Radiograph shows low density near the inner wall,
what is acceptance criteria for excess penetration as per ASME B 31.3 code, Please clarify the IMAGE CONTRAST GRAPH method .

Regards,

K.Sundar Rajan

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0ff884e9-b935-45ca-b277-d69e2324f37b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOwU13vQexX%3DOepA_d-7cPvLT2qtovFrg-bMSp2oGCfKDZ_rKA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...