Wednesday, February 18, 2015

Re: [MW:22890] Excess penetration measurment in Radiograph

There is no direct method to measure the magnitude of excess penetration on small bore closed butt welds. 

 

The possibilities to get conclusion are as below.

 

1. Highly skilled RT film interpretation expert can give proper feedback. 

2. Keep mock up test pieces of welder along accepted RT films and compare these films with the production joint RT films. You may get some input.

3. Boroscope may be used to get an idea of internal penetration of the production weld. For small bore there could be limitation while turning probe/cable/camera tip.


Regds/Jignesh


On Wednesday, 18 February 2015 12:54:50 UTC+5:30, George Dilintas wrote:

On my opinion extreme low density at the root area could be an indication of excess penetration.
The most reliable method to measure excess penetration is UT thickness measurement

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for sundarrajan kumaraswamy ---18/02/2015 05:04:58---  How to measure the excess penetration from the Radsundarrajan kumaraswamy ---18/02/2015 05:04:58---  How to measure the excess penetration from the Radiograph of  Small bore piping  DWDI superimpose

From: sundarrajan kumaraswamy <ksraja15@gmail.com>
To: materials-welding@googlegroups.com
Date: 18/02/2015 05:04
Subject: [MW:22887] Excess penetration measurment in Radiograph
Sent by: materials-welding@googlegroups.com





  How to measure the excess penetration from the Radiograph of Small bore piping  DWDI superimpose Radiograph shows low density near the inner wall,
what is acceptance criteria for excess penetration as per ASME B 31.3 code, Please clarify the IMAGE CONTRAST GRAPH method .

Regards,

K.Sundar Rajan

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to
materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/0ff884e9-b935-45ca-b277-d69e2324f37b%40googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b1960e6b-c44b-4e7b-b248-0b7567da60b9%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...