Re: [MW:22841] Dissimilar thickness weldment

I have a different opinion on this issue. My question to Mr. Shokri will be to confirm where is this macro from, if it is from WPQR qualification, to confirm where the PQR will be applicable to. The show macro is a typical macrographic report of a 6GR welding procedure qualification for welding of TYK joints in tubular connection for examples in Jackets, Bridges Boat landing etc. this type of qualification is preceeded by a tubular mock-up

Rems Okonkwo
IWE Nigeria

On Mon, Feb 9, 2015 at 1:18 PM, Sergio Antonio Muñoz Pinzón <seanmup@gmail.com> wrote:
That is a poor join desing, please see fig. 2.6 for good transition thickness designs

Sergio Muñoz
IWE-IIW
http://Weld-ING.blogspot.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c049d0f8-1ae0-4309-bcd1-8f4f0b3266f8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEpWm6tkvmN0Fkqr9hfxRuX1Oa-KFZ%2BAYjboixsqgqH%3D5WC76Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...