[MW:22872] PQR for carbon steel with S'S lined

Dear experts,
I have a situation I have to weld CS with SS lined pipe to CS with SS lined elbow.
CS pipe 10"/21.9mm with S'S clad 3mm internally
Pwht required, impact test not required.
Code of qualification- SEC IX & ASME Div II requirements.
Request you all to please advise on possible PQR qualification scenarios.

Thanks
Irfan

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADXGqGQxi3-Q2OW_Sa5OhZ4oraEDBYnd-MVtR1Z4JFix12AHKA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...