Wednesday, January 28, 2015

Re: [MW:22771] GTAW + SMAW

Using AWS  code NO. Using ASME  yes you have to write a new WPS  for single process.


Sent from Samsung Mobile


-------- Original message --------
From: Jay Poojary <jayogini@gmail.com>
Date:28/01/2015 17:05 (GMT+08:00)
To: materials-welding@googlegroups.com
Cc:
Subject: [MW:22769] GTAW + SMAW

Dear Experts,

Please clarify. If I have qualified a procedure with combination process i.e GTAW+SMAW for groove joint, then using this procedure can I allow to weld fillet joints using SMAW.



cordially,
Jay Poojary

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAcO%3DyToxo3L--R8LjJ4aFCc2zrx8Yvo%2BE%2BMPFwzw%3DW8JLhZwQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...