Monday, January 26, 2015

[MW:22757] How i can chose filler metal for resistance crorrosion overlay metal 42CrMo (standard GB 3077-88).

Dear Experts,
I have question about overlay for Roller of Cement with repair (Because corrosion). Base metal is 42CrMo - GB 3077-88, Diameter 1800mm   
I want ask you how to chose filler metal? and procedure (i think FCAW will be good). And how to test and check after welding?
Thanks you!

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c960ff61-60fe-4099-ac02-0fca2f728901%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...