Thursday, January 8, 2015

[MW:22684] Crack in fillet weld between Inconel 625 and superduplex steel (25 Cr)

Hello

 

I have a problem of crack in fillet weld between Inconel (ASTM B446 UNS N06625, 50 mm) and super-duplex steel (ASTM A182 F55, 35 mm). 

The crack is always in root pass. It seems to be hot-cracking. The welding process is the GTAW and the consumable use is an Inconel.

 

Many solutions were implemented to avoid crack:

1) First trial was perform with an ER NiCrMo 13 consumable

2) Second trial was perform with an ER NiCrMo 3 consumable

3) For Third trial, the welding sequence was change, the root pass was perform by alternate quarter to minimize the strength in the weld during the cooling

 

The dilution was controlled, the min preheat temperature was 60° and the max inter-pass temperature was 150°C.


Could you help me to solve this problem?







--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ca0f8a38-65c5-4994-bd2e-c8138c0966d9%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...