RE: [MW:22644] Corrosion Resistance Overlay process (CRO)

 
Pls. refer QW - 453

 

Date: Wed, 24 Dec 2014 11:29:18 -0800
From: yogeshpawar5@gmail.com
To: materials-welding@googlegroups.com
Subject: [MW:22634] Corrosion Resistance Overlay process (CRO)

Dear Expert,

As I have to prepare Welder certificate(WPQ) for Corrosion Resistance Overlay process (CRO) I need help for following things

1) Base metal Thickness Qualification Range for Plate,& Pipe
2) Weld deposit Thickness
3) Position
I have used 6mm Thk C.S. plate & Made overlay up to 5mm with S.S. electrodes in 1G position  no groove configuration in plate
welder can qualify for groove & fillet weld ? Which ASME Sec IX clause refer for these please advice

Thanks & Regards
Yogesh P.
 




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...