Friday, December 19, 2014

Re: [MW:22610] TG-X flux core TIG rod

Gents, there are GTAW flux cored filler rods on the market. This is used in situations where purging is not practical. The flux in the filler creates the gas to shield the weld pool. This does leave a deposit of slag on the root run. If you are doing a weld where the root is inaccessible for grinding or chipping, the only way to clean the root run is by chemical means as advised previously.


Sent from Samsung Mobile
-------- Original message --------
From: Umar Makrani
Date:19/12/2014 5:02 PM (GMT+02:00)
To: materials-welding@googlegroups.com
Subject: Re: [MW:22608] TG-X flux core TIG rod

TIG probably is mistyped FCW(flux cored welding) he might mean MIG. 

 

 

Thanks & Regards

 

Firoz Ahmed R. Makrani, PMP®

Sr. Inspection Engineer

 

Description: Description: Description: Applus Velosi Logo

 

M: +965 60409440 / 9990 5922

T: +965 2398 6464/6446/6556

F: +965 2398 3443

E: firoz.makrani@applusvelosi.com

www.applusvelosi.com

Address: Block 9, Building 24, Office 21, Ground Floor, East Ahmadi Industrial Area

P.O Box 1589, Salmiya-22016, Kuwait

Click here for ApplusVelosi's Email Disclaimer

Description: safety_head_600X90_velosi its coming

 

 

 

 


On 18 Dec 2014, at 17:51, M.R.Kolahkaj <kolahkaj@gmail.com> wrote:

Buddy...Slag by GTAW process.... You sure?

On Dec 17, 2014 10:14 PM, "Pravin Poornachandran" <htcispravin@gmail.com> wrote:
Dear Expert,

I'm having issue on removing slag on root pass welding for stainless steel pipe welding

Welding condition:
Material: SS 316L
Thickness: 4-5mm
Bevel angle: 65 deg
Root opening: 3-4mm
Root face: 1mm
Pipe dia: 4 inch

I'm using KOBELCO TG-X316L FCW TIG rod, special consumable which can eliminate back purging which save cost on Ar.

However, it is difficult to remove slag on inside the pipe.

Kindly advice if anyone have experience using TG-X from KOBELCO and how to remove the slag inside the pipe.

Best regards,
Pravin Poornachandran

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...