Re: [MW:22406] 2 images in 1 film , X-ray

Dear sir,

its need to inform you that i think there is some scattered radiation are seen, Rejected.

On Fri, Nov 28, 2014 at 9:23 PM, tugrulhan özdemir <tugrulhan9@gmail.com> wrote:
Dear Experts


6"   Dia ,  9,53mm   thickness   pipe,  X-Ray method RT performed . Two images of same pipe   found at the time of evaluation. I wonder is that acceptable or not?

Photo of film is attached with this mail


Regards


Tugrulhan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER
AUTHORIZED WELDING / NDT / PAINTING INSPECTION PERSONNEL,
AWS - CWI , CSWIP 3.1
BGAS  Gr 2 / 3
NDT II -UT , RT , MT , PT, VT

Pray for others, sometime, You might never need to pray for yourself again.....

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...