[MW:22352] RE: 22351] PQR -For P1-G1 TO G2

Hi Hasin,
 
You require a separate PQR to weld P1GR2 material on the basis of the existing PQR (P1Gr1 material).
Gr no is an essential variable for impact. Based on the contract or project specifications, sometimes one may have qualify PQR on the exact grade/specification etc.
 
However as a smart strategy, if one qualifies all the PQR's with P1 material with Gr1 -Gr2 combination most of the ASME code's welding requirements get well accounted for.
 
Thanks.
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Specialist
Ontario, Canada
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of hasin shaikh
Sent: Monday, November 24, 2014 11:05 PM
To: materials-welding@googlegroups.com
Subject: [MW:22351] PQR -For P1-G1 TO G2

Dear Expert

I have query about PQR P1-G1 To P1-G2 ,

we have already PQR for P1-G1,now group number is different and also have Impact requirement,so is it mandatory to perform PQR for G1 to G2? please suggest .,

--
*With Regards
Shaikh.Hasin
Email: hasin.shaikh@gmail.com
Mobile: +91-9924562942*


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...