[MW:22147] Re: PQR mentioning position 3G and our WPS stated 1G

Dear All,
Kindly advise,

1G Qualificaiton is mentioned on WPS & PQR and if we want to qualify the welder on 6G position, do we need to prepare new WPS and PQR or only PQR and WPS (1G) be the same....

Khan.... 

On Tuesday, November 16, 2010 11:27:05 AM UTC+4, israr wrote:
Dear,
You just delete position 1 g from wps and write All,
As per ASME Section IX if WPS is qualified in any one position of 1G
to 6G it is qualify for all the position.
Then u can attached nos of PQR with dirrent position following the
same WPS.

Regards
Israr Ahmed
Tata Projects Ltd.India
+919930308261

On Nov 11, 2:35 pm, Zulfan <zul...@insing.com> wrote:
> Dear all,
>
> please advice in our PQR mentioning position 3G and our WPS stated 1G
> is the WPS able to apply or need to run again PQR again?
> code ASME sec IX
>
> Thank
> zul

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...