Dear,
You should ďont worry about location , just be sure and instruct your lab that your sample shall not be less than 6.4 mm by 6.4 mm (80% of actual thickness) .otherwise you have to apply temperature correction .location shall be weld metal , HAZ are mandatory.in addition to that Generally we conducted the base material adjacent to HAZ to verify the base material impact properties.be sure that you should understand the temperature correction table of UG 84 with the help of some senior person .after that you will never find any problem in future .if your shop is U stamp certified than no one can explain u this table efficiently other than a Authorised Inspector.

Intekhab Alam Ansari
Lead Engineer QA/QC
RIL J3 Expansion Project
MTF/RTF Area
   

On 11 Sep 2014 21:15, "Mhaskar Aly" <mhaskar.aly@gmail.com> wrote:

Kindly advise size and location of impact test specimen for HAZ for 8mm PQR test coupon.

In table UG84.6, it said 1/4t to 1/2t single side, what does it mean.

Is this mean that specimen should be between this, then specimen size will be 2mm.

Two side weld it said middle 1/2t, what will size & location of HAZ specimen.

Pls advise

Ali

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...