Kindly need your advice to clear one issue based on Welder Qualification.? These questions were asked to me yesterday in Aramco Interview.

  • If a welder is qualified with CS, can he weld SS.? ( i answered he cannot as F4 and F5 doesn't allow as per ASME Sec IX), but the interviewer told me it can be welded in GTAW with some kind of Gas i forgot the name of it. but i have gone through all the reference code i dont find any as P number and F number are essential variable.

  • Welder requires tack welding qualification in ASME Sec IX or AWS D 1.1.? As per ASME Sec IX all the welders need to be qualified. As our company manufactures only Tanks and Vessels not much involved with AWS D 1.1, is there any applicable stuff where specifically welder needs to be qualified for Tank welding if he is not qualified welder.??

  • If a welder is qualified with ASME Sec IX, can he weld the jobs with the code based on AWS D 1.1.? I have answered yes it's possible as the requirements need to be followed, i.e., Essential variable, Client approval as per AWS D 1.1 Clause 4.2.2.1
 
Regards
Dhanabal Jalachandran

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...