Re: [MW:21429] Acceptance for Crack in plate

You can repair by welding. The repair method must be accepted by the A.I
Best regards
Dr Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
HBS Regional Technical Manager


  From: "Ali Varmazyar" [AV-ssg@msa.ir]
  Sent: 07/20/2014 04:16 PM ZE3B
  To: <materials-welding@googlegroups.com>
  Subject: [MW:21426] Acceptance for Crack in plate


Dear All

 

Hi,

We are a question in my Company. We buy an plate for P.V.

But we find some crack in it.

What code of ASME take about this matter?

 

 