Monday, June 23, 2014

[MW:21240] Product Marking as per SA 106 of ASME Sec. IIA, Ed. 2013.

Dear Experts,

Refering to Cl. No. 25 of SA 106 of ASME Sec. IIA, Ed. 2013, Pipe Length shall be marked in feet and tenths of a foot [meter to two decimal places] but no one reputed pipe manufacturer mark the length of pipe on pipes. Does it really require? If require, then I think it is an NC and shall have to close before use.

Further, what shall be the reason for not allowing/ accepting the latest edition/ addenda (2011a) of ASTM/ ASME in Table II-200-1? For eg., if we refer 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...