Saturday, May 31, 2014

Re: [MW:20938] Cathodic protection

If you are talking about Sacrificial anodes it will be no effect as we can use it underwater so Rain is no thing

Regards,
H.A


On Saturday, May 31, 2014 9:45 AM, 'Asif Shahzad' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Dear Expert what is effect of rain on cathodic protection 
 
Regards,

Engr.Asif Shahzad
+966591268872/+923007389793

B.E Chemical Engineering
API 510
CSWIP 3.1
BGAS LEVEL II
Lead Auditor QMS(9001-2008)
NEBOSH IGC
OSHA
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...