Thursday, May 29, 2014

[MW:20929] 1/2" Ball Valve 1500# Hydrotesting

Dear all,

I have query regarding of hydro testing 1/2" ball valve 1500#. It is possible to do testing?. Connection for ball valve 1 part threaded type and another part socket weld type. It is possible to waive the testing?. Advice me details reference code need to be applied and method of testing. Thank you in advance.

Mohd Firdaus Abd Rahim
QA/QC
+60122796361

Sent from my iPhone

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...