Saturday, April 26, 2014

Re: [MW:20680] Ladle(heat )analysis VS Product Analysis

Dear Mr. Payem,

You will have to refer particular product specification/ applicable code.

Thanks & regards,


C. R. GANDHI


From: C.Muni <cmkfc07@gmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Friday, April 25, 2014 7:26 PM
Subject: Re: [MW:20679] Ladle(heat )analysis VS Product Analysis

Dear Mr.Payem,
You refer ASTM A703 Latest edition.

Regards,


 Chithiran  Muniyanndi,MBA(ISM),PGDCA,PDQM,
Surveyor/Auditor,
Residential Office:
DNV Business Assurance India P Ltd,
29A,Postal Colony,Vicky Nivas,
Off MTP Road,Backside of KSB Pumps,
Narasimhanaickenpalayam PO,
Coimbatore 641031.
Tamilnadu,South India.
Mobile:99947 65591

Growth is the only evidence of life.


On Fri, Apr 25, 2014 at 10:07 AM, PAYAM MAFAKHER <pmafakher@gmail.com> wrote:
Would you please help me ,What is the Tolerance/Deviation in composition BetweenLadle(heat )analysis VS Product Analysis ?
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...