Hi Mr. Alam, 
If he is qualified with 2 " all GTAW only and didnt use this process for 6 months. Then the qualification is expired. But if within 6 months he use the process even on fillet welds only, then the qualification is still valid. But if he weld fillet welds using other process even the same welder, qualification still expired.
You have to come out with evidence like rt report or visual insp. report.


gulrez alam <gulrezhhi@gmail.com> wrote:
Dear experts

Can you explain to me .if any welder is qualified 6 month before with 2 " pipe .but this 6 month the welder is doing only fillet weld .

so i want to know this welder qualification is renew on his continue welding or need to retest.


Best regards 

G.Alam

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...