[MW:19952] Re: Welding consumable for A516 Gr.70 (Storage Tank) and PWHT issues

As i say, this is not pressure vessel.this is storage tank.

i asked to contractor about this situtation and finally i got information.

Design code : ASME Sec. VIII Div. I

Tank pressure : OPEN TO ATMOSPHERE !!!!!

Design Temperature: 50 Celcius

Wind Design Code ASCE-7 98/02/05/IBC-03/STS-1

Basic Wind Speed [V] 146.00 km/hr

Surface Roughness Category C: Open Terrain

Importance Factor 1.5

---

im confused !! design code asme sec viii but this is storage tank and open air !!!

how i can solve pqr and pwht issues ???



 








--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...