Dear Maghroud
For tests mentioned by Mr. Zarrinnaghsh, you have to care about radius of mandrel for bend test.

Regards


On Tue, Nov 26, 2013 at 2:01 PM, Kian <kzarrinnaghsh@gmail.com> wrote:
Dear Maghroud
Tension Test , 2 Specimens
Bend Test, 2 Root Bend/ 2 Face Bend or 4 Side bend specimens
در سه‌شنبه 26 نوامبر 2013، ساعت 12:06:13 (UTC+3:30)، Maghroud Moussa نوشته:
I have to qualify a WPS for A luminium welding. The informations are:
 
1- Material: 1050A  (SB209)
2- MIG Process
3- Filler metal: ER1100 (Diameter is 1.2mm)
4- Butweld joint, Thickness is 10.97mm
 
Please tell me what mechanical tests should i release for this speimen according to ASME IX.
 
Thanks
 
MAGHROUD Moussa
Welding Engineer
ETTERKIB.Spa

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...