Sunday, November 24, 2013

Re: [MW:19356] SUS304 Materials for Jib crane Rails Accessories

SUS304 and SS304 same 

Yes u cane use as mention WPS (316) 

Filler metal only changes use 308

Regards, 

Vidhyapathi 

On 24 Nov, 2013, at 6:04 pm, hany alfy <hanyon_alfy@yahoo.com> wrote:

Dear All

we have one job for Jib crane Rails Accessories the required Grade is Drawings is SUS304

I Believe this SS304 please Confirm am right or no?

If we have WPS/PQR for SS316 it can be used for this SS304 or no?

If now can you send me WPS for welding SS304?

Regards,
H.A

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...