[MW:19369] Cracking of Fire Proofing near Tie Rod in Spherical Gas Holder

Dear Friends,
 
In a recent inspection of Spherical Gas Holder, we observed cracking near the tie rods in the fireproofing layer at the junction of column and tie rod.
There were 16 columns supporting the gas holder and similar cracking was observed at all the locations.
 
(Please find the pics of cracks attached)
 
What may be the possible reason for the cracking?
 
Can anyone suggest where can we find assessment criteria to determine the criticality of the cracking?Which code/standard specifies the acceptance criteria for this?
 
Thanks & Regards
Eswar Raju.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...