RE: [MW:19110] Change in Supplementary Essential Need re-qualification?

Yes if THERE IS NO Impact test required.

 

Thanks,

HEMANT SUTHAR

IWT

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of george.dilintas@gr.bureauveritas.com
Sent: 29 October 2013 14:28
To: materials-welding@googlegroups.com
Subject: Re: [MW:19108] Change in Supplementary Essential Need re-qualification?

 

Yes it does

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor
API 510 Inspector
Prelude FLNG ASME Subject Matter Expert

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS HELLAS

Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Korea cell phone: +82 10 2777 8922


Ezat Adel ---29/10/2013 10:57:21---Dear Experts, i need your clarify that the changes in material group number with the

From: Ezat Adel <ezatadel2008@gmail.com>
To: materials-welding <materials-welding@googlegroups.com>
Date: 29/10/2013 10:57
Subject: [MW:19105] Change in Supplementary Essential Need re-qualification?
Sent by: materials-welding@googlegroups.com





Dear Experts,

i need your clarify that the changes in material group number with the
same p number need another welding qualification or not.

my case i have WPS for A312  grade TP 316, P no. 8 , group no. 1 to itself.
it's right to use it to weld  A312  grade TP 310s, P no. 8 , group no.
2 to itself.

Ezzat

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...