Wednesday, October 30, 2013

[MW:19134] REQUIREMENT OF PTC

Dear experts,

At presently i am working on a single equipment which construction code is ASME SEC. VIII DIV. 2

Details are as follows:
Shell Material:- SA 765 GR IV
Dish Material:-  SA 537 CL. 2
Cladding:- 5 mm (308L)

Thickness:-
Base material:- 133 mm

MDMT 0°C

My question is that i need PTC[Production Test Coupon] or not ??
If yes then How many??

My shell is forged shell so Long seam is not applicable in equipment.

Please Help me over this topic with help of Clause no. of Div.

Regards,
Ankit Gandhi
asgandhi.90@gmail.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...