Re: [MW:18777] Distance between welds toes to weld centerline

Hi,
Understand from your query that you are not able to maintain the minimum distance of 150mm between the reinforced plate and the Vertical Seam.
In my opinion
You would have to refer to 5.7.3.4 and figure 5.9 and maintain the minimum spacing as specified in fig 5.9 (a) (c) (e), which ever is applicable and do the RT accordingly.
 
If you have a different opinion, please let me know, I would be willing to learn.
 
Thanks and Regards
Rudolf

From: Mervin <mervin_kid@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Wednesday, 25 September 2013, 16:16
Subject: [MW:18768] Distance between welds toes to weld centerline

Dear expert,


Could you please help me what is the other option if the spacing showing in the attached drawing is not achive. There is no paragrap also mentioned in this case in api650.

Regards,

Mervin Dio
Qw welding insp.
Ssa.




Sent from my iPhone
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...