[MW:18757] Simulation test coupon & Production impact test coupon

Dear All,

Design Data
Code :ASME SEC VIII Div 1
Design Temperature:427 Deg C
Design Pressure:44 Kg/cm2
MDMT :O Deg C
PWHT: Required
Impact test: Required for all pressure part material
ASME Certification: Yes With U designation
MOC:SA 387 GR 12 CL2
Thickness:: Shell:12 mm,Head:18 mm.

1.Please advice whether Simulation test coupon & production impact test coupon (PTC) as per UG-84 (i) is required?
2.Is pressure part includes Fasteners?
3.Is there any flow chart/charts available to decide on PTC for carbon steel & alloy steel material?
4.Is separate post forming heat treatment is required as % extreme fiber elongation exceeds 10%

Thanks & Regards.
Prasanna

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...