Dear Raj,
 
Your Welding Engineer is right. As per code we don't need to qualify separate weld repair procedure, but at the same time please check client fabrication procedure. If it is mentioned separately to qualify the  procedure then follow-up TPI instructions.
 
Best Regards,
 
Jaywant 

On Wed, Aug 21, 2013 at 5:37 PM, raj susi <rjsusi@yahoo.com.sg> wrote:

Dear Experts

Good evening.
In our company we have some repairs to be done and we dont have repair procedures separately.
But we only follow the NCR disposition made by welding engineer. Which has some instructions to follow ie removal of defect, same wps to be used as per production weld, nde to be done as per job scope.
So now our TPI is asking for separate repair procedure.

In my previous company we did have separate repair procedures. But here we dont have any.

Our welding engineer is telling us that our repair is before PWHT and therefore we dont need a repair procedure separately.

Is it a must that we Should really have repair procedure ( whether before or after PWHT)?

THANKS
raj

Sent from Yahoo! Mail on Android

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...