[MW:18272] weld interruption

Dear Friends,

What is the percentage of weld interruption in pipeline butt weld? and
Where is mention about weld interruption any code or standard or specification?

In my project (Gas Pipeline) they are mention following statement about weld interruption in the project specification.

Welding shall continue until at least 2 filler passes have been completed.In the event of stoppage due to weekends, holidays and inclement weather, incomplete welds other than restrained Tie-in welds may be left for more than 48 hours provided that at least two fill passes have been completed.

Lawrence.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...